9 Operation

Depending on the CHANGE button settings and the use of "Crater repeat", torch operation varies as follows.
Note:
After turning on the torch switch, if the voltage detect is not executed, the welder goes in an error state (Err6: Arc
start error) and turns off the output automatically.

9.1 Welding current calibration

Welding current is tested and calibrated with following welding wire extension. it may need read justment with
moved welding parameters such as torch angle, wire type, shieling gas and other welding conditions.
Welding current
Extended wire length (Tip-Base
metal distance)
9.2 "NO CRATER"
Operation: Turn the torch switch on and off to start and stop welding arc respectively.
Operation
50A
0.9
wire
12
0.8
wire
1.2
wire
15
1.0
wire
38
100A
150A
200A
12
12
15
15
15
18
250A
300A
350A
18
18
22
25