SMALL SCRATCHES THAT CANNOT BE BUFFED OUT

1.
Thoroughly clean the affected area and then dry.
2.
Using 240 grit or finer sandpaper, lightly sand scratch to feather edges. Finish sand scratch with 320 grit or finer
paper to remove gloss from surface. Sand as little body surface as possible beyond scratch. See following
CAUTION.
CAUTION
• Be careful not to sand completely through the finish to the body material. If the finish is sanded
through and the thermo plastic olefin (TPO) body material is exposed, refer to Gouges, Punctures,
Tears, Large Scratches, and Abrasions on page 4-3.
3.
Using the brush provided with the touch-up paint (available from the Service Parts Dept., see following color
chart), apply paint to the scratch. Multiple layers of paint may be required to fill the scratch.
4.
Allow paint to dry completely (approximately 10-20 minutes), then lightly buff the imperfection.
5.
Apply wax to the entire body part to restore luster and weather protection.

TOUCH-UP PAINT COLOR CHART

COLOR
Beige
White
Red
Gray
Dark Gray
Royal Blue (Pacific Blue)
Black
Dark Green
Classic Blue (Navy)
Burgundy

GOUGES, PUNCTURES, TEARS, LARGE SCRATCHES, AND ABRASIONS

Touch-up is not recommended. Replace the entire body part or have it repaired by a professional paint and body repair
shop with experience repairing TPO bodies.
2009-2010 HUV 4214, HUV 4414, and HUV 4414X Maintenance and Service Manual
PART NUMBER
101997201
101997202
101997203
101997204
101997205
101997206
101997207
101997209
101997211
101997212
4
Front Body Repair
Page 4-3

Hide quick links:

Advertisement

Table of Contents
loading

Table of Contents